How Resistance Spot Welding Works: Process, Equipment and Uses

Resistance spot welding joins overlapping sheet metal with a short, high current pulse and electrode pressure. Learn the cycle, equipment, limits and uses.

On this page
  1. The short answer
  2. The principle
  3. Equipment
  4. The weld cycle
  5. Key parameters
  6. Materials and thickness
  7. Common defects and testing
  8. Where spot welding is used
  9. Advantages and limits

The short answer

Resistance spot welding joins overlapping metal sheets by squeezing them between two electrodes and passing a short pulse of high electric current through the stack. Resistance to the current is highest where the sheets touch, so that spot heats and melts into a small molten pool called a nugget. When the current stops, the electrodes keep pressing while the nugget cools and solidifies, fusing the sheets. No filler metal, flux or shielding gas is normally needed.

The principle

Heat from electrical current follows the relationship heat = current squared times resistance times time. Because spot welders use very high current for a very short time, and because the interface between the sheets has higher resistance than the copper electrodes and the bulk metal, the heating is concentrated exactly where the weld is needed. Water-cooled copper alloy electrodes carry the current in and draw heat away from the surface, which keeps the outer faces of the sheets from melting.

Equipment

  • Power source and transformer. Converts supply power into low voltage and very high current at the electrodes, often thousands of amps. Portable or small units may use other means, such as capacitor discharge or battery power.
  • Electrodes. Copper alloys are used for conductivity and strength. Tip shape and size help set the size of the weld.
  • Electrode holders and arms. Carry current and force; arm length and shape limit what parts can be reached.
  • Force mechanism. Pneumatic, hydraulic or servo systems apply pressure; small hand tools use a lever or spring.
  • Controller. Sets current, time and sequence.
  • Cooling. Water cooling is common on production machines.

Types include stationary pedestal welders, portable gun-type welders hung from a rail or carried by robots, and small hobby or battery-tab welders.

The weld cycle

  1. Squeeze. The electrodes close on the sheets and build up the set force before any current flows.
  2. Weld. Current flows for a very short time, often fractions of a second, forming the nugget.
  3. Hold. The current stops but the electrodes keep pressing while the nugget solidifies.
  4. Off (release). The electrodes open and the part moves to the next spot.

Many controllers add extra steps, such as upslope, downslope or a pulse sequence, to handle coated or thicker materials.

Key parameters

Quality depends on a few variables that interact:

  • Weld current. Too low gives a small or weak nugget; too high can cause expulsion, where molten metal is squeezed out as spatter.
  • Weld time. Longer times add heat, but too long can overheat and cause indentation.
  • Electrode force. Affects contact resistance and keeps the molten metal contained.
  • Electrode tip condition. Tips mushroom and wear with use, increasing contact area and lowering current density, so they must be dressed or replaced.
  • Surface condition. Scale, oil, paint and coatings change the resistance. See preparing metal for welding.

Settings come from the equipment maker’s charts, industry standards or weld trials on scrap.

Materials and thickness

Spot welding works best on thin sheet, commonly in the range of well under a few millimeters per sheet. It is widely used on low-carbon steel, stainless steel and nickel strip. Galvanized (zinc-coated) steel is spot welded often, but typically needs higher current and more electrode maintenance. Aluminum is possible but demands higher current and careful control because of its conductivity. Very thick sections generally call for other processes, such as those in welding processes and equipment.

Common defects and testing

  • Undersized or cold nuggets: from low current, short time or poor fit-up.
  • Expulsion: from excess current or poor contact.
  • Surface cracks or heavy indentation: from too much force, time or current.
  • Electrode sticking: from worn tips or coatings.

Production shops often check welds with peel or chisel tests, where a sample is torn apart and the nugget size is checked, along with ultrasonic testing or other non-destructive methods where required.

Where spot welding is used

  • Automotive body-in-white assembly, where a vehicle can have thousands of spots
  • Appliances, enclosures and other sheet metal products
  • Battery pack assembly, where nickel strips are joined to cells
  • Metal furniture and shelving
  • Light repair work on car body panels

Advantages and limits

Advantages: fast cycle times, no consumables like filler or gas, low skill needed once set up, easy to automate, and little distortion compared with arc welding.

Limits: lap joints only, with access needed from both sides; welds are discrete points, not a continuous seal; and the process suits thin sheet. For a sealed continuous joint made with the same principle, see seam welding. Spot welds also have less strength in peel loading than in shear, so joint design matters (see the basic weld joints).