What the 6G test is
The 6G test is a welder qualification test for groove welds on pipe. The pipe coupon is held at a fixed angle of about 45 degrees to horizontal and is not rotated, so the welder has to weld the whole joint in one fixed position. As you go around, the weld passes through flat, vertical and overhead orientations. This makes it widely regarded as one of the most demanding standard pipe tests.
The “G” stands for groove weld. For how 6G compares with 1G, 2G and 5G, see pipe welding positions.
What passing qualifies you for
Under many codes, a pass in 6G on a pipe coupon qualifies the welder for groove and fillet welds in all positions on pipe, and often on plate, within the limits of the other variables on the test. These variables include the process, filler metal, pipe diameter range and thickness range. The exact range is set by the governing standard, such as ASME Section IX, AWS D1.1, API 1104 or another code, and by the procedure. The documents involved are explained in what WPS, WPQ and PQR mean.
Be aware that:
- A qualification is tied to a process and set of variables. Passing with stick does not qualify you for TIG, for example.
- Employers and codes can also set a time limit, and continuity requirements to keep a qualification current.
- Some employers run their own tests even if you hold a certificate from elsewhere.
Typical test setups
Test details vary by employer, test center and code, but you may see:
- Pipe size. Often 2 inch or 6 inch nominal pipe, in a thick wall such as Schedule 80 or Schedule 160, or an extra-heavy wall.
- Process. Stick (SMAW), commonly with a 6010 open root and 7018 for fill and cap, or TIG (GTAW) for root, fill and cap. Some tests are combined, such as a TIG root with a stick fill and cap.
- Joint. A V-groove with a bevel in the area of 30 to 37.5 degrees per side, a small root face (or none, depending on the process), and a root gap in the range of about 1/16 to 1/8 inch. See pipe fit-up for how this is set up.
- Tacks. A few tacks, usually feathered at the ends.
Ask the test provider for the specific test procedure ahead of time, so that you know the process, material, thickness and any restrictions on cleaning or grinding.
How the test is evaluated
The finished coupon is inspected in stages, according to the code:
- Visual inspection. Looks at the cap profile, undercut, overlap, porosity, cracks and consistency. A weld that fails visually is normally rejected without further testing.
- Mechanical testing. Strips are cut from the coupon and bent in a guided-bend test. Root and face bends check for cracks and lack of fusion. Nick-break tests are sometimes used.
- Radiography. Some tests use X-ray in place of, or in addition to, bend tests.
Test fees vary a lot between providers, and sometimes include materials and sometimes do not. Practice coupons and consumables are an added cost, so plan ahead. How to become a certified welder covers the steps and costs.
Why welders fail
Common reasons include:
- Poor root fusion or lack of penetration, often caused by an uneven gap or a rushed root pass
- Burn-through or excess root convexity or concavity
- Lack of fusion between passes or at the groove sidewalls
- Slag inclusions from poor cleaning between passes
- Undercut at the cap edges
- Porosity from poor shielding gas coverage, damp electrodes or contaminated metal
- Stray arc strikes on the pipe outside the joint, which some codes treat as defects
- Not following the WPS, for example using the wrong electrode or amperage range
How to prepare
- Practice the exact test. Use the same pipe size, wall, process and position. Cut up your practice welds and bend-test them yourself.
- Master fit-up. A consistent bevel, gap and feathered tacks make the root easier. Practice setting up coupons repeatedly.
- Work the position in sections. Many welders find the overhead area at the bottom and the transitions at 3 and 9 o’clock the hardest. Practice these areas until you are comfortable.
- Keep consistent heat. Adjust your electrode or torch angle as the pipe curves, while keeping travel speed steady.
- Learn from your failures. Note where problems appear on the clock and what caused them.
- Know your electrode. If you are testing with stick, understand when and why 7018 might be used instead of 6010 at the root. See can you use 7018 for a root pass?
- Get fit and comfortable. Practice in the same gear you will wear on the test, including hood and gloves, and plan how you will sit or kneel at the position.
Tips for test day
- Read the test instructions carefully and ask questions before you start.
- Check your machine settings on a scrap piece first, if allowed.
- Do not rush the root pass. A good root usually makes the rest of the weld go more smoothly.
- Clean between every pass, even if you feel pressed for time.
- Take your time with the cap, and keep the width and height uniform.
- If something goes wrong partway through, ask whether the test rules allow repairs or grinding out and restarting. Do not assume.
For the full process, see the pipe welding process from root to cap, and for process choices, see what type of welding do pipe welders use?