What WFS means
In welding, WFS stands for wire feed speed: how fast the wire is pushed out of the MIG gun. It is usually measured in inches per minute (IPM) on US machines and in meters per minute (m/min) on many others. Some machines show a dial with no units, in which case a feed speed chart or a quick test is needed.
Why WFS matters: it controls amperage
On a typical MIG machine, the power source holds voltage steady and lets the current rise or fall as needed. The wire is melted at the arc, so the faster you feed it, the more current the machine has to supply to burn it off. In practice:
- Higher WFS means more amperage, more heat and deeper penetration, and more filler going into the joint.
- Lower WFS means less amperage and a cooler, shallower weld.
That is why most MIG setup guides suggest setting WFS first. Voltage then fine-tunes the arc.
How to set WFS step by step
- Identify your material thickness, wire diameter and gas. For example, mild steel, 0.030” or 0.035” solid wire, and C25 shielding gas. See good MIG settings for starting values.
- Use a chart as a starting point. The chart inside the machine door, or a manufacturer’s chart, will suggest a WFS and voltage. Treat it as a first guess rather than a final answer.
- Set the WFS to the suggested value. If your machine has no readout, pick a mid-range setting and adjust from there.
- Set voltage to the suggested value.
- Run a short bead on scrap of the same thickness, in the same position as the real joint.
- Adjust WFS in small steps until the bead looks right, then re-check the voltage.
Signs your WFS is too low or too high
Too low:
- The arc seems to burn back toward the tip, or the wire melts into a ball before touching the work.
- The bead is thin and flat, with little penetration.
- Burn-through is less likely, but you may see cold, poorly fused welds.
Too high:
- The wire stubs into the work and pushes the gun back.
- A loud, harsh crackle and a lot of spatter.
- The bead piles up tall and narrow.
- Burn-through on thin metal.
The symptoms can overlap with voltage problems, so change one setting at a time.
Balancing WFS with voltage
Think of WFS as the heat and deposition control, and voltage as the arc length and bead-shape control. A common description of a good short-circuit MIG arc is a steady sizzle, often compared to frying bacon.
- If the arc is crackling and stubbing, the voltage may be too low for the WFS, or the WFS too high for the voltage.
- If the arc is long, spattery and wandering, the voltage may be too high.
When you raise WFS considerably, expect to raise voltage a little as well. When you lower WFS, voltage often needs to come down.
What happens if travel speed is too fast?
Travel speed, one of the five essentials of welding, also changes the result even when WFS and voltage are right. If you move too fast:
- The bead becomes narrow and thin, sometimes “ropey.”
- Penetration and fusion drop, so the weld may not bond well to the side of the joint.
- You can get undercut, a groove melted into the base metal beside the weld that the filler does not fill.
- Porosity can become more likely in some situations, because the pool freezes quickly.
Moving too slowly has the opposite problem: too much heat in one place, a wide, heavy bead and possible burn-through. If you struggle to find the right pace, try adjusting WFS slightly instead of forcing your hand speed.
Other things that change the right WFS
- Wire diameter. Thinner wire needs a higher feed speed to carry the same current as thicker wire.
- Shielding gas. Pure CO2 generally needs slightly higher voltage than a 75/25 argon/CO2 mix; see the MIG shielding gas guide.
- Position. Vertical-up welds typically call for a lower WFS to control the pool.
- Stickout. Keeping stickout (the length of wire protruding from the tip) short and consistent, around 3/8” to 1/2” for smaller wires, helps keep current stable. Long stickout reduces current at a given WFS.
- Wire type. Metal-cored and flux-cored wires have their own manufacturer ranges.
If the arc is unstable or you see holes in the bead, the cause may not be WFS at all; check porosity in MIG welds.
Quick reference
WFS values depend on wire size, thickness and machine, so check the wire manufacturer’s chart or your machine’s chart. Our article on good MIG settings lists approximate starting ranges for common mild steel thicknesses. For the wider picture of how the process works, see MIG and TIG welding.