The short answer for mild steel
For general MIG welding of mild steel with solid wire, the most common choice is C25: 75% argon and 25% CO2. It gives a stable arc, moderate spatter and a good-looking bead on a wide range of thicknesses, and it is available from most gas suppliers. 100% CO2 is a cheaper alternative with deeper penetration, but it generally produces more spatter and a rougher arc.
What shielding gas does
The gas flows from the gun nozzle and surrounds the arc and molten pool, keeping out oxygen, nitrogen and moisture from the air. Without proper shielding, the weld can become porous and weak; see porosity in MIG welds. The gas also affects:
- how the arc behaves and how much it spatters,
- how deeply the weld penetrates,
- the shape of the bead,
- the voltage needed for a stable arc.
C25 (75% argon / 25% CO2)
- Best for: general mild-steel welding, especially thinner and medium material, and short-circuit transfer.
- Pros: smooth arc, lower spatter than CO2, good control and appearance.
- Cons: costs more than CO2, and penetration is a bit less deep than with straight CO2.
100% CO2
- Best for: budget-conscious work on thicker steel where appearance is secondary.
- Pros: inexpensive, deep penetration, tolerant of some surface imperfections.
- Cons: more spatter, a harsher arc and a flatter, less polished bead. It generally needs slightly higher voltage (around 1 V more is a common suggestion) than C25 on the same job.
Other argon/CO2 mixes
You may see mixes with less CO2, often sold as C20, C15, C10 or “98/2” argon/CO2 or argon/oxygen blends. Mixes with more argon are commonly used for higher-current work such as spray transfer and for stainless steel, and they tend to give a smoother arc and less spatter. They need enough current to run properly and may not suit small hobby machines. Check the wire manufacturer’s recommendation for your wire.
100% argon: for aluminum, not steel
Pure argon is the standard MIG gas for aluminum. On carbon steel, pure argon generally causes an erratic arc and poor penetration, so avoid it unless the wire or application specifically calls for it. Also note that “MIG” is short for metal inert gas, but on steel most setups use active gases such as CO2, which is why the process is sometimes called MAG. See our MIG and TIG overview for naming.
Gas choices by metal
| Metal | Common gas choices | Notes |
|---|---|---|
| Mild steel | C25 (75/25) or 100% CO2 | C25 is the usual all-round choice |
| Stainless steel | Argon-rich mixes (often with a small amount of CO2 or oxygen) or tri-mix | Follow the wire maker’s guidance |
| Aluminum | 100% argon | Needs a suitable wire feed setup |
| Flux-cored (self-shielded) | None | Wire provides its own shielding |
| Flux-cored (gas-shielded) | Often C25 or 100% CO2 | Check the wire datasheet |
Flow rate and setup
Typical flow rates are often around 15–25 cubic feet per hour. Use a regulator with a flowmeter, set flow while the gas is running, and check the manufacturer’s guidance for your nozzle size.
- Too little flow leaves the pool exposed.
- Too much flow can cause turbulence that pulls air into the stream.
- Wind and drafts can blow gas away; shield the work area or use a different process outdoors, such as self-shielded flux-cored wire.
- Check hoses, fittings and the regulator for leaks (and see storing and securing gas cylinders), and make sure the nozzle and diffuser are free of spatter.
Gas and settings
Changing gas changes how the arc behaves, so you may need to adjust voltage and wire feed speed. See good MIG settings and wire feed speed for how to tune on scrap.
Flux-core wire and gas
Self-shielded flux-core wire does not need gas, which is why it is popular for outdoor work. Gas-shielded flux-core and metal-cored wire do need gas, and the datasheet normally names the recommended mix.