The short answer
2T and 4T are two ways a TIG welder can interpret the switch on the torch. The “T” stands for “touch” or trigger action.
- In 2T, you press and hold the switch to weld and release it to stop. Two actions: press and release.
- In 4T, you press and release to start, then press and release again to stop. Four actions, with no need to hold the switch while you weld.
Not every machine offers both, and the exact behavior varies by brand, so check your manual.
How 2T works
- Press and hold: gas pre-flow begins, the arc starts, and the current moves to your set welding amperage (through upslope, if you set one).
- Release: the current ramps down (if downslope is set), the arc stops, and gas post-flow continues to protect the hot tungsten and weld.
It is simple and direct. The torch switch effectively behaves like an on/off button for the whole weld.
How 4T works
- First press: gas pre-flow begins and the arc starts, often at a lower starting current.
- First release: the current ramps up to the main welding amperage. You can now let go of the switch and keep welding.
- Second press: the current ramps down toward the crater (end) current.
- Second release: the arc stops and post-flow continues.
On many machines the second press can hold the crater current for as long as you keep it pressed, which lets you fill the end crater before you let go. The behavior varies between machines.
2T vs 4T at a glance
| 2T | 4T | |
|---|---|---|
| Switch actions | Press and hold, then release | Press, release, press, release |
| Hold switch during weld | Yes | No |
| Start/crater current options | Often limited | Usually more flexible |
| Good for | Short welds, tacks, learning | Long welds, less finger fatigue |
When to use 2T
- Tack welds and short welds, where holding the switch is easy.
- Learning torch control, because the sequence is simple.
- Quick adjustments and restarts on small parts.
When to use 4T
- Long welds where holding a switch would be tiring.
- Tight spaces or welding positions where a foot pedal is awkward.
- Welds where you want a controlled start and crater fill, particularly on aluminum, where crater cracks are a concern. See how to TIG aluminum for beginners.
Opinion varies. Some welders prefer 2T for short runs and tacking, while others use 4T for almost everything. Try both on scrap and see what suits you.
What about a foot pedal?
A foot pedal (or a fingertip control on the torch) gives you continuous, real-time control of amperage. 2T and 4T are mainly used when you do not have a pedal, or when the job does not need real-time heat control. With a pedal plugged in, the machine usually switches to pedal control and the torch-switch modes may no longer apply. The same pedal skills are useful for jobs such as TIG welding chrome-moly tubing.
Settings that interact with 2T and 4T
- Pre-flow: a short burst of gas before the arc starts.
- Upslope: the time the current takes to rise to welding amperage.
- Downslope: the time the current takes to fall at the end.
- Crater or end current: the low current used to finish the weld.
- Post-flow: gas that keeps flowing after the arc stops to protect the tungsten and the cooling weld.
Settings are typically preset by default but can be adjusted. Tungsten care also matters; see choosing TIG tungsten.
Common mistakes
- Releasing the switch too early in 4T, which can stop the arc without filling the crater.
- Pressing again at the wrong moment, so the weld ends mid-bead.
- Forgetting post-flow, which can leave a blackened tungsten tip and an oxidized end to the weld.
- Using the wrong mode for the job, for example 2T for a long weld that tires your hand.
For the broader process, see MIG and TIG welding.